EN AW-6060 15 x 3 mm
EN AW-6060
Is suitable for anodizing, and has a high corrosion resistance and good for anodizing. The alloy is suitable for welding.
We are not liable for items out of stock. The specified weight is theoretical. Please contact us if you have any further enquiries.
Alloys
Density | Si | Fe | Cu | Mn | Mg | Cr | Zn | Ti | Other | |||||
---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|
Name | g/cm3 | Min | Max | Min | Max | Max | Max | Min | Max | Max | Max | Max | Max | Rest |
EN AW-6060 | 2.7 | 0.3 | 0.6 | 0.1 | 0.3 | 0.1 | 0.1 | 0.35 | 0.6 | 0.05 | 0.15 | 0.1 | 0.15 | Al, Aluminium |
Aluminium Properties
Thermal conductivity | Coefficient of thermal expansion | Melting point | Elastic modulus | Electrical conductivity | |||
---|---|---|---|---|---|---|---|
Alloy | Temper | W/m*K | µm/(m*K) | min °C | KN/mm2 | %IACS | |
EN AW-6060 | O | 23.4 | 610 | 655 | 69 | ||
EN AW-6060 | T1 | 195 | 23.4 | 610 | 655 | 69 | 49.5 |
EN AW-6060 | T4 | 187 | 23.4 | 610 | 655 | 69 | 48 |
EN AW-6060 | T5 | 209 | 23.4 | 610 | 655 | 69 | 54 |
EN AW-6060 | T6 | 209 | 23.4 | 610 | 655 | 69 | 54 |
Mechanical properties
Dimension | Tensile strength (Rm) MPa | Proof stress (Rp0,2) | Elongation | Brinell Hardness | Elongation A50mm | ||||
---|---|---|---|---|---|---|---|---|---|
Norm | Alloy | Temper | Min | Max | Rm N/mm2 | MPa | % min | HBS | % min |
EN 755-2:2013 | EN AW-6060 | T6 | - | 5 | 190 | 150 | 8 | 70 | 6 |
EN 755-2:2013 | EN AW-6060 | T6 | - | 15 | 190 | 150 | 8 | 70 | 6 |
EN 755-2:2013 | EN AW-6060 | T6 | 5 | 25 | 170 | 140 | 8 | 70 | 6 |
EN 755-2:2013 | EN AW-6060 | T66 | - | 15 | 215 | 160 | 8 | 75 | 6 |
EN 755-2:2013 | EN AW-6060 | T66 | - | 5 | 215 | 160 | 8 | 75 | 6 |
EN 755-2:2013 | EN AW-6060 | T66 | 5 | 25 | 195 | 150 | 8 | 75 | 6 |