ATP 101

Material id: 1149877

Profile System properties

  • Weight : 5.23
  • Profile Name: ATP 101 - 2500 mm
  • Length: 2500.0 mm

EN AW-6082

Has a high strength and a good corrosion resistance. The alloy is good for welding, and you can anodize it. 


We are not liable for items out of stock. The specified weight is theoretical. Please contact us if you have any further enquiries.

Alloy - Alloys

Si
Min
0.7
Max
1.3
Fe
Min
-
Max
0.5
Cu
Min
-
Max
0.1
Mn
Min
0.4
Max
1
Mg
Min
0.6
Max
1.2
Cr
Min
-
Max
0.25
Zn
Min
-
Max
0.2
Ti
Min
-
Max
0.1
Others
Min
0.15
Max
-

Alloy - Aluminium Properties

Alloy
EN AW-6082
Temper
O
Thermal conductivity
W/m*K
216
Coefficient of thermal expansion
µm/(m*K)
23,1
Annealing
Min
-
Annealing
Max
-
Melting point
Min
575
Max
650
Melting point
Max
650
Elastic modulus
KN/mm2
70
Electrical conductivity
%IACS
55,5
Alloy
EN AW-6082
Temper
T1
Thermal conductivity
W/m*K
-
Coefficient of thermal expansion
µm/(m*K)
23,1
Annealing
Min
-
Annealing
Max
-
Melting point
Min
575
Max
650
Melting point
Max
650
Elastic modulus
KN/mm2
70
Electrical conductivity
%IACS
-
Alloy
EN AW-6082
Temper
T4
Thermal conductivity
W/m*K
167
Coefficient of thermal expansion
µm/(m*K)
23,1
Annealing
Min
-
Annealing
Max
-
Melting point
Min
575
Max
650
Melting point
Max
650
Elastic modulus
KN/mm2
70
Electrical conductivity
%IACS
42
Alloy
EN AW-6082
Temper
T5
Thermal conductivity
W/m*K
-
Coefficient of thermal expansion
µm/(m*K)
23,1
Annealing
Min
-
Annealing
Max
-
Melting point
Min
575
Max
650
Melting point
Max
650
Elastic modulus
KN/mm2
70
Electrical conductivity
%IACS
-
Alloy
EN AW-6082
Temper
T6
Thermal conductivity
W/m*K
172
Coefficient of thermal expansion
µm/(m*K)
23,1
Annealing
Min
-
Annealing
Max
-
Melting point
Min
575
Max
650
Melting point
Max
650
Elastic modulus
KN/mm2
70
Electrical conductivity
%IACS
44