ATP 163

Profile System properties

  • Weight : 2.58
  • Profile Name: ATP 163 - 6000 mm
  • Length: 6000.0 mm

EN AW-6060

Is suitable for anodizing, and has a high corrosion resistance and good for anodizing. The alloy is suitable for welding.


We are not liable for items out of stock. The specified weight is theoretical. Please contact us if you have any further enquiries.

Alloy - Alloys

Si
Min
0.3
Max
0.6
Fe
Min
0.1
Max
0.3
Cu
Min
-
Max
0.1
Mn
Min
-
Max
0.1
Mg
Min
0.35
Max
0.6
Cr
Min
-
Max
0.05
Zn
Min
-
Max
0.15
Ti
Min
-
Max
0.1
Others
Min
0.15
Max
-

Alloy - Aluminium Properties

Alloy
EN AW-6060
Temper
O
Thermal conductivity
W/m*K
-
Coefficient of thermal expansion
µm/(m*K)
23,4
Annealing
Min
-
Annealing
Max
-
Melting point
Min
610
Max
655
Melting point
Max
655
Elastic modulus
KN/mm2
70
Electrical conductivity
%IACS
-
Alloy
EN AW-6060
Temper
T1
Thermal conductivity
W/m*K
195
Coefficient of thermal expansion
µm/(m*K)
23,4
Annealing
Min
-
Annealing
Max
-
Melting point
Min
610
Max
655
Melting point
Max
655
Elastic modulus
KN/mm2
70
Electrical conductivity
%IACS
49,5
Alloy
EN AW-6060
Temper
T4
Thermal conductivity
W/m*K
187
Coefficient of thermal expansion
µm/(m*K)
23,4
Annealing
Min
-
Annealing
Max
-
Melting point
Min
610
Max
655
Melting point
Max
655
Elastic modulus
KN/mm2
70
Electrical conductivity
%IACS
48
Alloy
EN AW-6060
Temper
T5
Thermal conductivity
W/m*K
209
Coefficient of thermal expansion
µm/(m*K)
23,4
Annealing
Min
-
Annealing
Max
-
Melting point
Min
610
Max
655
Melting point
Max
655
Elastic modulus
KN/mm2
70
Electrical conductivity
%IACS
54
Alloy
EN AW-6060
Temper
T6
Thermal conductivity
W/m*K
209
Coefficient of thermal expansion
µm/(m*K)
23,4
Annealing
Min
-
Annealing
Max
-
Melting point
Min
610
Max
655
Melting point
Max
655
Elastic modulus
KN/mm2
70
Electrical conductivity
%IACS
54