EN AW-5052

Width

1000.0 mm

Weight

250.0 kg

Thickness

0.63 mm

We offer coils in the standard thickness from 0.63 mm to 1 mm. We deliver all our coils in the standard width of 1000 mm and basic, we can deliver in three standard sizes: 250 kg, 500 kg and 1000 kg. If you request further information or other dimensions - you are welcome to contact us.


  • Width: 1000.0 mm
  • Weight: 250.0 kg
  • Thickness:
  • Weight: 250kg
  • Weldability: High
  • Corrosion: High
  • Cut/drilling: Medium
  • Surface: Medium
On request

EN AW-5052

It is easy processing and has a high corrosion resistance and good for welding. The alloy is not suitable for decorative anodising. 


We are not liable for items out of stock. The specified weight is theoretical. Please contact us if you have any further enquiries.

Alloy - Alloys

Si
Min
-
Max
0.25
Fe
Min
-
Max
0.4
Cu
Min
-
Max
0.1
Mn
Min
-
Max
0.1
Mg
Min
2.2
Max
2.8
Cr
Min
0.15
Max
0.35
Zn
Min
-
Max
0.1
Others
Min
0.15
Max
-

Alloy - Aluminium Properties

Alloy
EN AW-5052
Temper
Hx2
Thermal conductivity
W/m*K
138,0
Coefficient of thermal expansion
µm/(m*K)
23,7
Annealing
Min
-
Annealing
Max
-
Melting point
Min
605
Max
650
Melting point
Max
650
Elastic modulus
KN/mm2
70000
Electrical conductivity
%IACS
35,0
Alloy
EN AW-5052
Temper
Hx4
Thermal conductivity
W/m*K
138,0
Coefficient of thermal expansion
µm/(m*K)
23,7
Annealing
Min
-
Annealing
Max
-
Melting point
Min
605
Max
650
Melting point
Max
650
Elastic modulus
KN/mm2
70000
Electrical conductivity
%IACS
35,0
Alloy
EN AW-5052
Temper
Hx6
Thermal conductivity
W/m*K
138,0
Coefficient of thermal expansion
µm/(m*K)
23,7
Annealing
Min
-
Annealing
Max
-
Melting point
Min
605
Max
650
Melting point
Max
650
Elastic modulus
KN/mm2
70000
Electrical conductivity
%IACS
35,0
Alloy
EN AW-5052
Temper
Hx8
Thermal conductivity
W/m*K
138,0
Coefficient of thermal expansion
µm/(m*K)
23,7
Annealing
Min
-
Annealing
Max
-
Melting point
Min
605
Max
650
Melting point
Max
650
Elastic modulus
KN/mm2
70000
Electrical conductivity
%IACS
35,0
Alloy
EN AW-5052
Temper
Hx9
Thermal conductivity
W/m*K
-
Coefficient of thermal expansion
µm/(m*K)
23,7
Annealing
Min
-
Annealing
Max
-
Melting point
Min
605
Max
650
Melting point
Max
650
Elastic modulus
KN/mm2
70000
Electrical conductivity
%IACS
-
Alloy
EN AW-5052
Temper
O
Thermal conductivity
W/m*K
138,0
Coefficient of thermal expansion
µm/(m*K)
23,7
Annealing
Min
-
Annealing
Max
-
Melting point
Min
605
Max
650
Melting point
Max
650
Elastic modulus
KN/mm2
70000
Electrical conductivity
%IACS
35,0